Beta-Ti bcc-superalloys, comprising an A2 beta-Ti matrix reinforced by ordered intermetallic B2 beta-prime-TiFe precipitates, exhibit an unusual recrystallisation that occurs with no externally applied strain (i.e. no thermomechanical processing). Thermal ageing at 750 degrees Celsius for 72 h results in refinement of the grain size from 364 um to 30 um. This grain refinement is driven by discontinuous precipitation of beta-prime-TiFe lamellae with the beta-Ti matrix from grain/phase boundaries, which is associated with significant misorientation and increased dislocation density, attributed as precipitation induced recrystallisation (PIX).